Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 9.00 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 °C
9.00 µin/in-°F

@Temperature 68.0 °F
Performance Alloys MoldStar® 18 (PAS 18) Bronze Mold Alloy
Description: MoldStar® 18 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: SlidesGibsWear PlatesMold Locking DevicesSl..
CTE, linear 16.2 µm/m-°C

@Temperature -40.0 - 149 °C
9.00 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PAI T5030 Polyamide-imide, glass reinforced, extruded (ASTM Product Data Sheet)
CTE, linear 16.2 - 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
9.00 - 12.0 µin/in-°F

@Temperature 140 - 280 °F
Average value: 18.6 µm/m-°C Grade Count:6
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
CTE, linear 16.2 µm/m-°C

@Temperature 21.1 - 102 °C
9.00 µin/in-°F

@Temperature 70.0 - 215 °F
Materion ToughMet® T2 CX 90
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
CTE, linear 16.2 µm/m-°C

@Temperature 25.0 - 500 °C
9.00 µin/in-°F

@Temperature 77.0 - 932 °F
Wieland Porta Maximum NF PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 715 Copper Nickel 30%, 1/4 Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 715 Copper Nickel 30%, Extra Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 715 Copper Nickel 30%, Spring
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 735 Nickel Silver 18%, 3/4 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 735 Nickel Silver 18%, Extra Spring
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 735 Nickel Silver 18%, Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 735 Nickel Silver 18%, Spring
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 752 Nickel Silver 18%, Extra Spring
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info..
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 762 Nickel Silver 12%, Extra Hard
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 762 Nickel Silver 12%, Extra Spring
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..
CTE, linear 16.2 µm/m-°C

@Temperature 100 °C
9.00 µin/in-°F

@Temperature 212 °F
CMW® 353 Copper Alloy
CMW® 353 material is an economical high strength, high conductivity copper base alloy. It is a heat treatable copper base alloy and its excellent properties are obtained largely through heat treatm..
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 °C
9.00 µin/in-°F

@Temperature 68.0 °F
California Fine Wire Nickel Alloy 60 Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
CTE, linear 16.2 µm/m-°C
9.00 µin/in-°F
Aremco Aremco-Bond™ 2340 High Temperature Epoxide Potting Compound
High Temperature, Low Viscosity, Low Expansion, High Glass Transition Temperature & Chemical Resistance
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 °C
9.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Copyright © lookpolymers.com All Rights Reserved