Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 27.0 µm/m-°C @Temperature -40.0 - 150 °C |
15.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E831 |
Quadrant EPP Semitron® MPR-1000 (ASTM Product Data Sheet) |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® AS-30CF/000 UV Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued Description/Features:Carbon Fiber ReinforcedUV StabilizedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy 13 Indium Solder Alloy Information Provided by Indium Corporation |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-2510 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-710 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | Through-Plane |
GrafTech eGRAF® SPREADERSHIELD™ SS500 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1/CF/15/HS Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy 12 Lead Solder Alloy Tin-free indium solderInformation Provided by Indium Corporation |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-1220 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
3.45 mm/mm; ASTM D696 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature -30.0 - 100 °C |
15.0 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
2.7 mm/mm; ASTM D696 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
3.45 mm/mm; ASTM D696 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Zelux® 20% GF Polycarbonate 20% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS179 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS186 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS240 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS295 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 27.0 µm/m-°C @Temperature -30.0 - 100 °C |
15.0 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature -30.0 - 100 °C |
15.0 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM C531 |
Chesterton ARC 791 Composite Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex.. |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi.. |
|||
CTE, linear | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Quantum Nylon 6/6 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermylon® LSG-440A 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
CTE, linear | 27.0 - 44.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 - 24.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL PX2938 PPE (Asia Pacific) PPE+PS GF20% High Heat FR V-0 |
|||
CTE, linear | 27.0 - 68.0 µm/m-°C @Temperature 125 - 175 °C |
15.0 - 37.8 µin/in-°F @Temperature 257 - 347 °F |
Average value: 37.4 µm/m-°C Grade Count:5 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |