Indium Corp. Indalloy 12 Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 12 Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tin-free indium solderInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 11.0 g/cc
0.397 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 9.0

@Load 100 kg,
Time 30.0 sec
9.0

@Load 220 lb,
Time 0.00833 hour
Tensile Strength at Break 39.5 MPa
5730 psi
Elongation at Break 23 %
23 %
Shear Strength 21.9 MPa
3180 psi
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 25.0 W/m-K

@Temperature 85.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 290 - 310 °C
554 - 590 °F
Solidus 290 °C
554 °F
Liquidus 310 °C
590 °F
Component Elements Properties Metric English Comments
Indium, In 5.0 %
5.0 %
Lead, Pb 90 %
90 %
Silver, Ag 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000310 ohm-cm
0.0000310 ohm-cm