Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 22.0 - 47.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 - 26.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Lexan® LC120 PC (Asia Pacific) |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-7938/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 50/CF/10/GF/20/BK Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | |
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-0797 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-0918/EM/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-0923/GY2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-8389/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy 240 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
CTE, linear | 22.0 µm/m-°C | 12.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
|
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
CTE, linear | 22.0 - 25.0 µm/m-°C | 12.2 - 13.9 µin/in-°F | |
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t.. |
|||
CTE, linear | 22.0 - 25.0 µm/m-°C | 12.2 - 13.9 µin/in-°F | |
Master Bond EP30ANHT Two Part, Electrically Isolating Epoxy Adhesive Description: Master Bond Polymer System EP30ANHT is a two part epoxy system with terrific thermal conductivity, while maintaining electrical insulation. One noteworthy property is its wide service t.. |
|||
CTE, linear | 22.0 - 25.0 µm/m-°C | 12.2 - 13.9 µin/in-°F | |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS205 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS235 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Zell-Metall Engineering Plastics Zellamid 1500T (PEEK modified) Zellamid® 1500 (Polyetheretherketone - PEEK, natural) is the registered trademark for Zell-Metalls semi-crystalline high performance thermoplastic which exhibits a unique combination of high m.. |
|||
CTE, linear | 21.9 µm/m-°C | 12.2 µin/in-°F | |
Hexcel® HexPly® F522 Epoxy Resin HexPly® F522 is an advanced, modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness, excellent hot-wet properties .. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 176 °F |
53752-A |
BASF Elastollan R 2001 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Glastic GLASGUARD Scuff and Bulkhead Liners GlasGuard Scuff and Bulkhead Liners serve as a method of protecting trailer walls from damage caused by forklift trucks and careless loading and unloading of freight. Manufactured of 1/4" thick fib.. |
|||
CTE, linear | 22.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |
|||
CTE, linear | 22.0 - 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 - 39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL PX2935 PPE+PS (Asia Pacific) PPE/PS, GF20%, non-FR |
|||
CTE, linear | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
|
AIM 97In/3Ag Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |