Polymer Property : CTE, linear = 53.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 30.0 - 53.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 29.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Lexan® LGK4010 PC (Asia Pacific)
CTE, linear 35.0 - 53.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
19.4 - 29.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Lexan® LGN1500 PC (Asia Pacific)
CTE, linear 29.0 - 53.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.1 - 29.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Lexan® LGN2000 PC (Asia Pacific)
CTE, linear 29.0 - 53.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.1 - 29.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Lexan® 3412 PC (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear 53.0 - 53.0 µm/m-°C

@Temperature 40.0 - 130 °C
29.4 - 29.4 µin/in-°F

@Temperature 104 - 266 °F
Average value: 53.0 µm/m-°C Grade Count:1
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..
CTE, linear 53.0 - 53.0 µm/m-°C

@Temperature 40.0 - 130 °C
29.4 - 29.4 µin/in-°F

@Temperature 104 - 266 °F
Average value: 53.0 µm/m-°C Grade Count:1
Overview of materials for Phenolic, Resole, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral Filled". Each property range of values reported is minimum and maximum values ..
CTE, linear 10.0 - 53.0 µm/m-°C
5.56 - 29.4 µin/in-°F
Average value: 31.7 µm/m-°C Grade Count:12
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
CTE, linear 29.0 - 53.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.1 - 29.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000 PC (Asia Pacific)
CTE, linear 30.0 - 53.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 29.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL PX2949 PPE+PS (Asia Pacific)
PPE+PS GF+Mineral Filler total 40%
CTE, linear 31.0 - 53.0 µm/m-°C
17.2 - 29.4 µin/in-°F
Average value: 41.3 µm/m-°C Grade Count:7
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..
CTE, linear 15.0 - 53.0 µm/m-°C

@Temperature 40.0 - 130 °C
8.33 - 29.4 µin/in-°F

@Temperature 104 - 266 °F
Average value: 29.6 µm/m-°C Grade Count:12
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..