CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Asia Pacific)
CTE, linear 40.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.2 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
CTE, linear 20.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.1 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Lexan® LCG0820 PC (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear 2.00 - 50.0 µm/m-°C
1.11 - 27.8 µin/in-°F
Average value: 23.8 µm/m-°C Grade Count:8
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
CTE, linear 22.0 - 50.0 µm/m-°C
12.2 - 27.8 µin/in-°F
Average value: 36.0 µm/m-°C Grade Count:3
Overview of materials for Polystyrene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Wood Filled". Each property range of values reported is minimum and maximum values of appro..
CTE, linear 12.0 - 50.0 µm/m-°C
6.67 - 27.8 µin/in-°F
Average value: 28.7 µm/m-°C Grade Count:33
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
CTE, linear 10.0 - 50.0 µm/m-°C
5.56 - 27.8 µin/in-°F
Average value: 25.9 µm/m-°C Grade Count:27
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
CTE, linear 35.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
19.4 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL S100G10 PPE+PS (Asia Pacific)
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL GTX CRN530 PPE+PA6 (Asia Pacific)
30%GF GTX grade for Non Auto market
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Noryl GTX GTX880 PPE+PA6 (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL GTX GTX6801 PPE+PA (Asia Pacific)
PPE+PA, GF 30%
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Noryl GTX GTX6801 PPE+PS+PA66 (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear 45.0 - 50.0 µm/m-°C
25.0 - 27.8 µin/in-°F
Master Bond EP30HV Optically Clear, High Strength Two Part Epoxy
Description: Master Bond EP30HV is a lower viscosity, two component epoxy system for high performance bonding, sealing, coating and potting. It is formulated to cure at room temperature or more rapi..
CTE, linear 40.0 - 50.0 µm/m-°C
22.2 - 27.8 µin/in-°F
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive
Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic..
CTE, linear 45.0 - 50.0 µm/m-°C
25.0 - 27.8 µin/in-°F
Master Bond UV10TKMed One component UV curable, biocompatible, high viscosity compound
Product Description: Master Bond UV10TKMed is a higher viscosity, one part UV system for bonding, sealing and coating that passes USP Class VI testing along with ISO 10993-5 for cytotoxicity. It has..
CTE, linear 45.0 - 50.0 µm/m-°C
25.0 - 27.8 µin/in-°F
Master Bond EP30M4 Chemically Resistant Two Component Epoxy System
Master Bond Polymer System EP30M4 is a two component epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weight. EP30M4 resi..
CTE, linear 45.0 - 50.0 µm/m-°C
25.0 - 27.8 µin/in-°F
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive
Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temper..
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
16.7 - 27.8 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BIF-11 Bonded (Composite) Magnetic Material
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
16.7 - 27.8 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BIF-17 Bonded (Composite) Magnetic Material
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
16.7 - 27.8 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BIF-19 Bonded (Composite) Magnetic Material
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
16.7 - 27.8 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BIF-2 Bonded (Composite) Magnetic Material
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
16.7 - 27.8 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BIF-16 Bonded (Composite) Magnetic Material
CTE, linear 36.0 - 50.0 µm/m-°C
20.0 - 27.8 µin/in-°F
Average value: 43.2 µm/m-°C Grade Count:5
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
CTE, linear 0.702 - 50.0 µm/m-°C
0.390 - 27.8 µin/in-°F
Average value: 29.7 µm/m-°C Grade Count:7
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
CTE, linear 20.0 - 50.0 µm/m-°C
11.1 - 27.8 µin/in-°F
Average value: 32.5 µm/m-°C Grade Count:19
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Copyright © lookpolymers.com All Rights Reserved