Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 99.0 µm/m-°C @Temperature -40.0 - 149 °C |
55.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Nylatron® GSM Blue Nylon, Cast Oil & MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
CTE, linear | 99.0 µm/m-°C @Temperature -40.0 - 149 °C |
55.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
CTE, linear | 99.0 µm/m-°C @Temperature -40.0 - 149 °C |
55.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
CTE, linear | 99.0 µm/m-°C @Temperature -40.0 - 149 °C |
55.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
|
North Wood Plastics HDPE with 20% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (DAM) Information provided by Ravago. |
|||
CTE, linear | 99.0 - 99.0 µm/m-°C @Temperature 22.8 - 55.0 °C |
55.0 - 55.0 µin/in-°F @Temperature 73.0 - 131 °F |
Average value: 99.0 µm/m-°C Grade Count:1 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 100 °C |
55.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
Technetics Group Amicon™ Nylon 6/66
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Multibase Multi-Flex® D 5308 848 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsInformation provided by Multibase |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Multibase Multi-Flex® D 5308 Platinum TPO Thermoplastic Polyolefin Elastomer Forms: PelletsInformation provided by Multibase |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Sta-Tuf High Impact Thermoplastic Alloy Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® Chemfilm® DF100 Fluoropolymer Cast Film Description: Used for Chemical Process, Electrical/Electronics, Medical, Protective/Decorative. Surface Treatments Available: Chemical Etching (1 or 2 sides). Information provided by Saint Gobain Pe.. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® Chemfilm® MR Fluoropolymer Cast Film Description: Commonly used for Aerospace/Release Film ApplicationsInformation provided by Saint Gobain Performance Products. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® Chemfilm® VB Fluoropolymer Cast Film Description: Commonly used for Aerospace/Release Film ApplicationsInformation provided by Saint Gobain Performance Products. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® FEP Fluoropolymer Film Features/Benefits:Outstanding clarityOutstanding anti-stick release propertiesPerformance from -254°C (-425°F) to 205°C (400°F)Exceptional chemical resistance and electric propertiesComp.. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 40.0 - 130 °C |
55.0 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 3554 Phenolic, Granular, Compression Molded PLENCO 03554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 03554 is available in black. It is UL listed. 03554 is a re-numbe.. |
|||
CTE, linear | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Diamond Polymers Centrex® 825 Sheet Extrusion Grade Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 22.8 - 55.0 °C |
55.0 µin/in-°F @Temperature 73.0 - 131 °F |
ASTM E831 |
Ensinger Tecaform™ MT Acetal, Medical Grade (POM) TECAFORM® MT is Ensinger's specially formulated medical grade acetal. The material is resistant to multiple cleaning and disinfection agents, and to a number of solvents. It can be steam sterilized.. |
|||
CTE, linear | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696, DIN 53 752, ASTM E831 |
Ensinger Tecaform™ SAN Polyacetal (POM) TECAFORM™ (Polyacetal) and TECAPRO™ SAN (Polypropylene), provide an additional safety factor in reducing incidence of bacterial contamination. The raw materials are charged with an antimicrobial .. |
|||
CTE, linear | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM E831 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |
|||
CTE, linear | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Cast Nylons Nycast® 12 Cast Nylon 12 NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical chara.. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
55.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8253 HS BK-102 PA6 (Dry) Ultramid 8253 HS BK-102 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying leve.. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
55.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8253 HS PA6 (Dry) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
55.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Lubri-Tech™ AT-000/15T-2S Copolymer Acetal - 15% PTFE, 2% Silicone Lubricated
(discontinued **) Data provided by PolyOne. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
|
Plenco 6554 Phenolic, Granular, Compression Molded
(discontinued **) Two-Stage Phenolic. PLENCO 06554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 06554 is available in black.Information supp.. |
|||
CTE, linear | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Quantum Acetal-Homopolymer Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® MFA Fluoropolymer Film Features/Benefits:Outstanding clarityPerformance from -254°C (-425°F) to 230°C (446°F)Outstanding flex life and stress-crack resistanceOutstanding anti-stick release propertiesExcellent electric.. |