Data provided by North Wood Plastics, Inc.
Physical Properties Metric English Comments
Density 1.003 g/cc
0.03624 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 2.6 g/10 min

@Temperature 190 °C
2.6 g/10 min

@Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.0 MPa
2180 psi
ASTM D638
Tensile Strength, Yield 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Tensile Modulus 1.70 GPa
247 ksi
ASTM D638
Flexural Yield Strength 31.0 MPa
4500 psi
ASTM D790
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.40 J/cm
2.62 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 99.0 µm/m-°C

@Temperature 20.0 °C
55.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ASTM D648
Flammability, UL94 HB
HB
0.32 cm x 1.25 cm x 12.5 cm sample
HB
HB
0.32 cm x 1.25 cm x 12.5 cm sample
Processing Properties Metric English Comments
Processing Temperature <= 200 °C
<= 392 °F
To prevent fiber degradation.