Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Sta-Tuf High Impact Thermoplastic Alloy Sign Grade Sheet

Category Polymer , Thermoplastic
Manufacturer Spartech
Trade Name Sta-Tuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Sta-Tuf High Impact Thermoplastic Alloy Sign Grade Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Sign Grade SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
ASTM D638
Flexural Yield Strength 57.2 MPa
8300 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Unnotched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 187 J
138 ft-lb
73°F; ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 99.0 µm/m-°C

@Temperature 20.0 °C
55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523