Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 68.4 µm/m-°C @Temperature -34.4 - -1.11 °C |
38.0 µin/in-°F @Temperature -30.0 - 30.0 °F |
ASTM D696 |
Plaskolite Vivak PETG Sheet VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details... |
|||
CTE, linear | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
|
RedEye On Demand Polycarbonate High Impact Strength & Temperature Resistant for Rapid Prototyping Polycarbonate (PC) is an actual industrial-grade thermoplastic that is impact-resistant and structurally strong. PC parts are built with a layered manufacturing process utilizing Fused Deposition Mo.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -18.0 - 38.0 °C |
38.0 µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
Plaskolite Polycarbonate Mirror Sheet Better strength, security, and flame resistance than PETG mirror sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
CTE, linear | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
Quantum Polycarbonate Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech PC-2000 High Impact Polycarbonate Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Sungard Ultra Weatherable Polycarbonate Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Stratasys® Polycarbonate A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts .. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Plaslube® PC-50/TF/13/SI/2 NAT Polycarbonate |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 201-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 2061-15 Polycarbonate CALIBREâ„¢ 2061-15 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 301-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4310-10 Polycarbonate EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4330-15 Polycarbonate EMERGEâ„¢ PC 4330-15 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4330-22 Polycarbonate EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4630-10 Polycarbonate EMERGEâ„¢ PC 4630-10 advanced resin is formulated to supply both excellent ultraviolet stability and enhanced ignition resistance while maintaining excellent physical properties and processabilit.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 301 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 303-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4310-15 Polycarbonate EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4330-6 Polycarbonate EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information .. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 - 82.2 °C |
38.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4600-10 Polycarbonate EMERGEâ„¢ PC 4600-10 advanced resin is formulated to supply both clarity and enhanced ignition resistance while maintaining excellent physical properties. Applications: Information Technology E.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Zelux® M Machine Grade Polycarbonate Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger Tecanat™ Unfilled Polycarbonate (PC) Tenacat™ is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps.. |
|||
CTE, linear | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM E831 |
Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature -40.0 °C |
38.0 µin/in-°F @Temperature -40.0 °F |
ASTM E831 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |
|||
CTE, linear | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice.. |
|||
CTE, linear | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 8302 Rigid PVC, Extrusion & Molding Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such .. |