Thermal Properties Metric English Comments
CTE, linear 68.4 µm/m-°C
38.0 µin/in-°F
ASTM D696
Quantum Polycarbonate
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech PC-2000 High Impact Polycarbonate Sign Grade Sheet
Description: Sign Grade SheetInformation provided by Spartech.
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Sungard Ultra Weatherable Polycarbonate Sign Grade Sheet
Description: Sign Grade SheetInformation provided by Spartech.
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech UltraTuf SG Polycarbonate Sheet
Description: Polycarbonate SheetInformation provided by Spartech.
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech UltraTuf SP-7010 Polycarbonate Sheet
Description: Polycarbonate SheetInformation provided by Spartech.
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Plaslube® PC-50/TF/13/SI/2 BK3585 Polycarbonate
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 201-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 201-10 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 201-22 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 2061-15 Polycarbonate
CALIBREâ„¢ 2061-15 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and..
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 2061-22 Polycarbonate
CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and..
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 301-10 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 301-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 4310-6 Polycarbonate
EMERGEâ„¢ PC 4310-6 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Equ..
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 4330-22 Polycarbonate
EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec..
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 4610-10 Polycarbonate
EMERGEâ„¢ PC 4610-10 advanced resin is formulated to deliver both outstanding clarity and enhanced ignition resistance while maintaining excellent physical properties and processability. Applica..
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 201-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 2060-6 Polycarbonate
CALIBREâ„¢ 2060-6 resin is designed for medical applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clarity..
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 2061-6 Polycarbonate
CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and ..
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 302-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 303-10 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron CALIBREâ„¢ 303-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 4310-15 Polycarbonate
EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Plaslube® PC-50/TF/13/SI/2 WT8966 Polycarbonate
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Zelux® W Window Grade Polycarbonate
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ensinger Tecanat™ Unfilled Polycarbonate (PC)
Tenacat™ is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps..
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Dow CALIBRE™ MEGARAD™ 2081-15 Polycarbonate
CALIBRE™ MEGARAD™ 2081-15 resin is specially formulated to meet the radiation sterilization needs of the healthcare industry, while providing exceptional clarity, heat resistance, impact strength..
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 °C
38.0 µin/in-°F

@Temperature -40.0 °F
ASTM E831
Arkema Group Solarkote® PB Acrylic
For PVC/acrylic alloys Information provided by Arkema Group
CTE, linear 68.4 µm/m-°C
38.0 µin/in-°F
ASTM D696
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice..
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 8302 Rigid PVC, Extrusion & Molding
Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such ..