Polymer Property : CTE, linear = 30.6 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C

@Temperature -40.0 - 149 °C
17.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PAI T4203 Extruded Polyamide-imide (ASTM Product Data Sheet)
CTE, linear 30.6 µm/m-°C

@Temperature -40.0 - 149 °C
17.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet)
This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis..
CTE, linear 30.6 µm/m-°C

@Temperature -40.0 - 149 °C
17.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet)
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N1040MGHL Nylon 6/6 (DAM)
Information provided by Ravago.
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (DAM)
Information provided by Ravago.
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM)
Information provided by Ravago.
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N2043L Nylon 6 (DAM)
Information provided by Ravago.
CTE, linear 30.6 - 37.8 µm/m-°C
17.0 - 21.0 µin/in-°F
Average value: 32.4 µm/m-°C Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep..
CTE, linear 30.6 - 59.4 µm/m-°C
17.0 - 33.0 µin/in-°F
Average value: 41.4 µm/m-°C Grade Count:3
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
CTE, linear 30.6 µm/m-°C

@Temperature -40.0 - 149 °C
17.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Semitron® 480 ESd PEEK, static dissipative, extruded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic ProductsThis PEEK based static dissipative material provides a dissipative range of 10E+6 - 10E+9 ohms/sq. Semitron® ESd 480 is very dimensionally sta..
CTE, linear 30.6 µm/m-°C

@Temperature -40.0 - 150 °C
17.0 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E831
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet)
CTE, linear 30.6 - 37.8 µm/m-°C
17.0 - 21.0 µin/in-°F
Average value: 35.4 µm/m-°C Grade Count:3
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Ensinger Sintimid™ V 40% graphite Polyimide (PI)  (discontinued **)
SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V..
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N1040MGL Nylon 6/6 (DAM)  (discontinued **)
Information provided by Ravago.
CTE, linear 30.6 - 60.0 µm/m-°C
17.0 - 33.3 µin/in-°F
Average value: 44.1 µm/m-°C Grade Count:5
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
ITW Devcon Metal Repair Ceramic Repair Putty, Dark Blue
Information provided by ITW Devcon
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
Trelleborg AEM Syntac® 350 Syntactic Foam
Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.Available in block, sheet and ro..
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
Trelleborg AEM Syntac® 351 Syntactic Foam
Syntac® 351 is a castable syntactic composite material of epoxy resin and high performance hollow glass microspheres designed specifically for molding thermoforming plugs and other associated tooli..
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
Trelleborg AEM Syntac® Eccolite® Ultra
Eccolite® Ultra is a new generation syntactic foam plug assist material, a new thermoplastic compound developed in response to the needs of the thermoforming industry. Eccolite® is tough and robus..
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Ensinger TECASON™ P MT Polyphenylsulfone (PPSU)
TECASON™ P MT is a polyphenylsulfone suited primarily to applications in the medical industry. It has improved performance in terms of temperature, impact strength and chemical resistance, as well..
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Ensinger TECASON™ P Polyphenylsulfone (PPSU)
TECASON™ P is a polyphenylsulfone that exhibits excellent temperature, impact and chemical resistance properties.
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
CMT Materials HYTAC® C Castable Syntactic Tooling
HYTAC-C is a one-part castable product in the HYTAC family of syntactics. This product is available as an uncured, single component mixture that may be poured or cast into a wide variety of shapes a..
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
RADEL® R is a Polyphenysulfone produced by Solvay Advanced Polymers. RADEL® R is in the same performance category as products like Polysulfone and ULTEM® (PEI). RADEL® R has increased performa..
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylon® NSG-730A 65% Ceramic and Glass Fiber Reinforced
Information provided by Asahi Thermofil
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
Trelleborg AEM Syntac® 450 Syntactic Foam
Syntac® 450 syntactic foam is the high temperature (450°F/232°C) member of the Syntac® product family.A rigid, high strength composite of epoxy resin and hollow glass microspheres, Syntac® 450 ..
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylon® NSG-440A 60% Ceramic and Glass Fiber Reinforced
Information provided by Asahi Thermofil
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Solvay Specialty Polymers Parmax® 1200 Self-Reinforcing Polyethersulfone  (discontinued **)
PARMAX 1200 self-reinforcing polymer (SRP) is an ultra-high performance amorphous, melt-processable engineering thermoplastic. The unique properties of this material are due primarily to the inheren..