Material Notes:
Eccolite® Ultra is a new generation syntactic foam plug assist material, a new thermoplastic compound developed in response to the needs of the thermoforming industry. Eccolite® is tough and robust, but also maintains the unique features and benefits of the other products in the Syntac® family. It is manufactured from a specially formulated thermoplastic resin and hollow glass microspheres. Unlike nylon-based materials Eccolite® Ultra boasts an exceptionally high temperature characteristic, maintaining its profile over extended operation cycle terms in service temperatures up to 392°F/200°CAll information provided by Trelleborg Emerson & Cuming
Physical Properties Metric English Comments
Density 0.737 g/cc
0.0266 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 74

@Temperature 220 °C
74

@Temperature 428 °F
Compressive Strength 68.9 MPa
10000 psi
Compressive Modulus 2.36 GPa
343 ksi
Izod Impact, Unnotched 0.721 J/cm
1.35 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
Specific Heat Capacity 1.46 J/g-°C
0.350 BTU/lb-°F
Thermal Conductivity 0.156 W/m-K
1.08 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Descriptive Properties Value Comments
Color White