Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 19.8 - 30.1 µm/m-°C @Temperature 20.0 °C |
11.0 - 16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Network Polymers Kepital® F20-25 Description: Natural Acetal Copolymer, 25% Glass Reinforced GradeInformation provided by Network Polymers Inc. |
|||
CTE, linear | 19.8 µm/m-°C @Temperature -40.0 - 150 °C |
11.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E831 |
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
CTE, linear | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Quantum PEEK 30% Carbon Filled Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 19.8 - 139 µm/m-°C | 11.0 - 77.2 µin/in-°F | Average value: 72.2 µm/m-°C Grade Count:46 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
CTE, linear | 19.8 µm/m-°C @Temperature -40.0 - 149 °C |
11.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet) |
|||
CTE, linear | 19.8 - 54.0 µm/m-°C | 11.0 - 30.0 µin/in-°F | Average value: 32.9 µm/m-°C Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
CTE, linear | 19.8 - 57.6 µm/m-°C | 11.0 - 32.0 µin/in-°F | Average value: 38.2 µm/m-°C Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
CTE, linear | 19.8 - 57.6 µm/m-°C | 11.0 - 32.0 µin/in-°F | Average value: 35.6 µm/m-°C Grade Count:5 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
GEHR Plastics Ultem 2300 PEI-30 GF 30% Glass Fiber Reinforced
(discontinued **) Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and great resistance. It's unique torque strength permits the econom.. |
|||
CTE, linear | 19.8 - 180 µm/m-°C | 11.0 - 100 µin/in-°F | Average value: 68.4 µm/m-°C Grade Count:29 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
CTE, linear | 19.8 - 41.4 µm/m-°C | 11.0 - 23.0 µin/in-°F | Average value: 27.0 µm/m-°C Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
CTE, linear | 19.8 µm/m-°C | 11.0 µin/in-°F | Average value: 19.8 µm/m-°C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 19.8 - 55.8 µm/m-°C | 11.0 - 31.0 µin/in-°F | Average value: 34.2 µm/m-°C Grade Count:29 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear | 19.8 - 30.0 µm/m-°C | 11.0 - 16.7 µin/in-°F | Average value: 22.5 µm/m-°C Grade Count:5 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear | 19.8 - 400 µm/m-°C | 11.0 - 222 µin/in-°F | Average value: 73.1 µm/m-°C Grade Count:13 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
CTE, linear | 19.8 µm/m-°C @Temperature 22.8 - 260 °C |
11.0 µin/in-°F @Temperature 73.0 - 500 °F |
ASTM E831 |
Saint-Gobain Meldin® 7022 DF Direct Formed Graphite Filled Polyimide Melidin® 7022 DF is a direct formed polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin® .. |
|||
CTE, linear | 19.8 µm/m-°C @Temperature 20.0 °C |
11.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Tempalux® 30% GF Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
CTE, linear | 19.8 - 170 µm/m-°C | 11.0 - 94.4 µin/in-°F | Average value: 88.1 µm/m-°C Grade Count:36 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
CTE, linear | 19.8 µm/m-°C @Temperature 20.0 °C |
11.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Lubri-Tech™ PI-30GF/15T Polyetherimide (PEI), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 19.8 µm/m-°C @Temperature 20.0 °C |
11.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® SF-35GF-25MN/000 L Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |