Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 110 - 200 µm/m-°C @Temperature 20.0 °C |
61.1 - 111 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Rotuba 856, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 60.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 140 °F |
|
Omnia Plastica Arnite Omnialite POM c Acetal Copolymer Polyoxymethylene, commonly called Acetal, is a crystalline polymer obtained from the polymerisation of formaldehyde. Discovered fairly recently (1960), it has enjoyed rapid growth and large acceptan.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
DN.53752 |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
CTE, linear | 110 µm/m-°C @Temperature -40.0 - 149 °C |
61.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ASTM E831 |
Lucite International Diakon® ST35G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
CTE, linear | 110 - 130 µm/m-°C | 61.1 - 72.2 µin/in-°F | |
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDC-4ND is a two component, very flexible epoxy system for high performance bonding, sealing and coating with a non-drip consistency. It has a one to four mix ra.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete a.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 307E4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
CTE, linear | 110 µm/m-°C | 61.0 µin/in-°F | ASTM D696 |
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM) TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | |
Hippe PP Polypropylene Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 360A4861301 Propionate Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® EB-08 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | DIN 52328 |
Isoflon PA 11 Polyamide 11 General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon. |
|||
CTE, linear | 110 µm/m-°C @Temperature -30.0 - 100 °C |
61.1 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifax™ CA186 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent paintability and paint durability, good processabi.. |
|||
CTE, linear | 110 - 130 µm/m-°C | 61.1 - 72.2 µin/in-°F | ASTM D696 |
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |