Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 48.0 °C | 118 °F | Tag Closed Cup |
LyondellBasell PNP Propylene glycol normal propyl ether Information provided by Lyondell. |
|||
Flash Point | 47.5 °C | 118 °F | |
Shandong Dongyue Polymer TFP Tetrafluoropropanol Usage: TFP is widely used on medicine, agrichemical, dyestuff and intermediate of fine chemical such as the color agent of photography, textile finishing agent, fluoropolymer assistant ingredient, d.. |
|||
Flash Point | 48.0 °C | 118 °F | closed cup |
Dow Corning Z-6106 SILANE Dow Corning® Z-6106 Silane acts as a coupling agent designed to promote adhesion of two dissimilar materials. It can be used to bond a polymeric coating or adhesive to an inorganic substrate or to .. |
|||
Flash Point | 48.0 °C | 118 °F | |
BASF Formic Acid - 99-100% Formula: CH2O2CAS: 64-18-6Description: Formic Acid 99-100% is a colorless to yellowish liquid, with a pungent odor. It is miscible with water and other organic substances in all proportion.Synonyms.. |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Flash Point | 48.0 °C | 118 °F | |
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating 840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body.. |
|||
Flash Point | 48.0 °C | 118 °F | |
Aremco Lamp-Coat™ LC4010-BT High Temperature Coating, Silicone Aluminum-filled coating for application over black top coated headlamps to 1020 °F (550 °C). |
|||
Flash Point | 48.0 °C | 118 °F | |
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC) |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Flash Point | 47.8 °C | 118 °F | |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |