Physical Properties Metric English Comments
Specific Gravity 0.887 g/cc
0.887 g/cc
20/20°C
Density 0.884 g/cc

@Temperature 20.0 °C
0.0319 lb/in³

@Temperature 68.0 °F
Solubility in Water 100 %
100 %
20°C
Viscosity 2.3 cP

@Temperature 25.0 °C
2.3 cP

@Temperature 77.0 °F
Molecular Weight 118.2 g/mol
118.2 g/mol
Vapor Pressure 0.00227 bar

@Temperature 20.0 °C
1.70 torr

@Temperature 68.0 °F
Evaporation Loss 22 %
22 %
n-BuAc=100%
Surface Tension 27 dynes/cm
27 dynes/cm
25°C
Thermal Properties Metric English Comments
Boiling Point 150 °C
302 °F
at 760 mmHg
Flash Point 48.0 °C
118 °F
Tag Closed Cup
Optical Properties Metric English Comments
Refractive Index 1.41

@Temperature 25.0 °C
1.41

@Temperature 77.0 °F
Descriptive Properties Value Comments
CAS Number 1569-01-3