Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | |
Plastcom SLOVALEN PC 59 GB 10 PP, 10% glass beads FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass beads and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ISO 75-1/-2 |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C @Temperature 200 °C, Time 14400 sec |
320 °F @Temperature 392 °F, Time 4.00 hour |
Annealed; ISO 75-f |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ASTM D648 |
Ravago Manufacturing Americas Enviramid™ N2340MGHL BK Post Consumer Recycle Nylon 6, 25/15% Glass/Mineral Filled Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ASTM D648 |
Kolon KOCETAL® GF305 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ISO 75-1,-2 |
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C @Thickness 3.20 mm |
320 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA12 CF13 L 13% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 13% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and lubricatedInformation provided by TP Composi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C @Thickness 6.40 mm |
320 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM DU242 PEI Enhanced low temperature impact, high flow Polyetherimide blend. ECO Conforming. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Valox® 508 PBT (Europe-Africa-Middle East) VALOX 508 is a 30% glass reinforced PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, distributor caps, ignition rotors, voltage regulator.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA4/6 HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA4/6 HS LBK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackTPCI# 9651150Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Asia Pacific) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK 150 Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ASTM D648 |
Techmer ES Plaslube® J-80/20/TF/15 NAT Acetal (POM) Copolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Europe-Africa-Middle East) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized, UV-Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ISO 75 |
Polyram RamTal PM3009G4 Polyacetal for Injection Molding, 20% Glass Fiber Reinforced 20% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 - 180 °C | 320 - 356 °F | ISO 75 Af |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® LV-3 ESD PA12-GF30 Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 - 291 °C | 320 - 555 °F | Average value: 281 °C Grade Count:70 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® LC-15H black PA12-CF15 Product description: Grilamid LC-15H black is a Polyamide 12 injection molding product reinforced with 15% carbon fibers. The product is inherently black and is only available in this color.Main Att.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C @Temperature 200 °C, Time 14400 sec |
320 °F @Temperature 392 °F, Time 4.00 hour |
ISO 75-f |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |