Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
PolyOne Lubri-Tech™ AT-000/20T Copolymer Acetal - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | |
MTI ThermoStran® PP-30G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® POM CO GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 15% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically Coupled and Low ExtractablesInformation provided by TP Composites, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO AF15 Availability: North AmericaForms: PelletsAdditive: Aramid Resin Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO CF10 TL10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated and CopolymerUL File: E157318Information provided b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-30FG-0790 30% Glass Fiber Reinforced, Impact Modified Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-30FG-0890 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-40FG-1804 40% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP LGF40 CC HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled and Heat StabilizedAppearance: Bla.. |