Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYblend 45V GF10 PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ASTM D648 |
PTS PCA-2010 Flame Retardant PC/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYlux 3809S F20 PC/PBT-Blend, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75-1/-2 |
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data) Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C @Thickness 3.20 mm |
212 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® TE5000SP PBT+PC Description: Injection Molding, PBT+PC, Low Gloss, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75-1/-2 |
Mitsubishi Xantar® C CF 407 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO TL10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | annealed; ISO 75-A |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75-1, 2 |
Polyplastics Duracon® M450-44/M450S Acetal Co-polymer (POM), Standard, Super high flow, High cycle DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75-1, 2 |
Polyplastics Tepcon M320 Acetal-copolymer (POM), High Fluidity, High Cycle Information provided by PolyPlastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75-1, 2 |
Polyplastics Tepcon M450 Acetal-copolymer (POM), Super High Fluidity, High Cycle Information provided by PolyPlastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75 |
Polyram PlusTek PA106 Nylon 66 for Injection Molding, with Molybdenum Disulfide Nylon 66 with molybdenum disulfide, low friction and high abrasion resistance, for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | DIN 53461 |
Polyram RamLloy PBB701 PC/ABS alloy, UV Stabilized UV stabilized PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | DIN 53461 |
Polyram PlusTek PA100 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75 |
Eurotec® Tecoform® PO20 NL RT POM, PTFE modified, natural Information provided by Eurotec® |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)
(Unverified Data**) Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75 -1 & -2 flat |
Asahi Kasei Tenac®-C 5520 Copolymer Acetal Resin Similar to TENAC®-C 4520 but with higher flow and minimized mold deposit.Information provided by Asahi Kasei Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ASTM D648 |
Asahi Kasei Xyron® 340V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75 |
BLUESTAR BS270 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75 -1 & -2 flat |
Asahi Kasei Tenac® SH410 Homopolymer Acetal Resin General purpose grade, high impact, high elongation, medium viscosityInformation provided by Asahi Kasei Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75-1, 2 |
Polyplastics Duracon® M140-44/M140S Acetal Co-polymer (POM), Standard, High flow DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics NORYL PX2355 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2355 is an unfilled, medium heat, low odour and low emission material with excellent heat aging performance. It has been developed for automotive interior applications, such as instrument pa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | |
Arkema Group Oroglas® V 825 T Acrylic
(discontinued **) OROGLAS V 825 T exhibits an excellent balance of properties including superior thermal resistance with an easy processing behavior.OROGLAS V 825 T is then the material of choice for automotive appli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ASTM D648 |
Chase Plastics CP Pryme® PPC100-35M Polypropylene Copolymer Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C @Thickness 6.40 mm |
212 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade Information provided by Samsung Cheil Industries. |