Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C @Thickness 3.18 mm |
155 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 2320 LCW Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C @Thickness 6.35 mm |
155 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding 87546 Polyvinyl Chloride, Rigid (PVC, Rigid) Provisional Data SheetInformation provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C @Thickness 3.18 mm |
155 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Nymax™ 1200 A Black 11 A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
RheTech Products T20P100-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
RheTech Products T20P100-248 20% Talc Reinforced Polypropylene, General Purpose Grey Applications: Durable goodsElectronics housingsHVAC ducts - air distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
RheTech Products T20P105-00FA 20% Talc Reinforced Polypropylene, FDA Compliant Components, Natural Applications: Food traysFood service implementsContainersConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1200THL BK Nylon 6/6 Available in North America Additive: Heat Stabilizer, Impact Modifier and Lubricant Features: Lubricated, Impact Modified and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation prov.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N2000HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
RheTech Products HP532-00 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Natural Applications: Interior trimCenter tail light bezelPackage trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
Polymer Resources NY66-IM2 Impact Modified Nylon 66 Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (DAM)
(discontinued **) Information provided by Entec. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
Spartech SP-3010 Rigid PVC Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GB30 30% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PP FR-N X Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D-648 |
Axiall 8240 Rigid PVC, Extrusion Georgia Gulf 8240 is a general-purpose rigid PVC extrusion compound designed for applications requiring the following properties: Rigidity/StiffnessGlossImpact Strength & ToughnessFlame RetardantCh.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C | 155 °F | Unannealed (0.250"); ASTM D648 |
LTL Color Compounds ColorFast® NY1 Nylon 6 Injection molding nylon 6, with or without lubeAll information provided by LTL Color Compounders, Inc. |