Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 45.5 MPa
6600 psi
ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Yield Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790
Izod Impact, Unnotched 7.47 J/cm
14.0 ft-lb/in
ASTM D256
0.267 J/cm

@Temperature -40.0 °C
0.500 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 42.0 J
31.0 ft-lb
73°F; ASTM D3029
10.8 J

@Temperature -40.0 °C
8.00 ft-lb

@Temperature -40.0 °F
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C
155 °F
ASTM D648
Flammability, UL94 V-0
V-0
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523