Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ISO 75/Method Af |
Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0242-U MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 - 83.0 °C | 102 - 181 °F | Average value: 66.5 °C Grade Count:34 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ASTM D648 |
Chevron Phillips K-Resin® CK02 Styrene-Butadiene Copolymer, Blow Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: CK02 is a blow molding SBC designed to provide a softer, tougher, more flexible container while retaining the clarity and gloss of bottles produced from.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | |
Teknor Apex TEKRON® 4300LM-P96-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ASTM D648 |
Chevron Phillips K-Resin® XK40 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: XK40 is an extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. Compared to KK38, KX40 offers.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | |
Covestro Desmopan® 460 Thermoplastic Polyurethane Desmopan 460 is a TPU on the basis of a special ester.Applications: Bearing shells, gear wheels, seals, cable connectors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience w.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ASTM D648 |
ExxonMobil LL 8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.9 °C | 102 °F | ASTM D648 |
ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.9 °C | 102 °F | ASTM D648 |
ExxonMobil LLDPE LLP 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ASTM D648 |
ExxonMobil LLP8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ASTM D648 |
ExxonMobil HD 6704.18 Injection Molding Resin Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ASTM-D648 |
Braskem RD34U3 LLDPE Rotomolding Polyethylene The resin RD34U3 is a linear low-density polyethylene, 1-butene based, with excellent processability and a good balance of stiffness and impact strength. It contains long term UV6 stabilization and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0242-UG MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 - 130 °C | 102 - 266 °F | Average value: 92.7 °C Grade Count:13 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | ASTM D648 |
ExxonMobil LL 8460 Rotational Molding Resin
(discontinued **) LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 °C | 102 °F | injection molded specimen; ASTM D648 |
Phillips Sumika Marlex® ABF-035 Thermoplastic Polyolefin
(discontinued **) Applications: Vehicle front-end air damsHigh impact exterior trimInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This produc.. |