Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips K-Resin® XK40 Styrene-Butadiene Copolymer, Sheet Grade

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer Chevron Phillips Chemical Company LP
Trade Name K-Resin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips K-Resin® XK40 Styrene-Butadiene Copolymer, Sheet Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene CopolymerCustomer Benefits: XK40 is an extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. Compared to KK38, KX40 offers greater polystyrene acceptance and better clarity.Applications: Major applications include thermoformed blister packs, cups and lids, and portion packages.Processing Recommendations:Extrusion: Melt Temperature, 218°C maximum. High shear and restrictive type screws tend to degrade the melt. Generally no need to dry resin.Specification Data: FDA Regulation 21 CFR 177.1640; suitable for food contact. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50.Data provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 15.2 MPa
2200 psi
2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Elongation at Break 330 %
330 %
2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Flexural Yield Strength 22.2 MPa
3220 psi
Test specimens were injection molded by ASTM D1897; ASTM D790
Flexural Modulus 0.696 GPa
101 ksi
Test specimens were injection molded by ASTM D1897; ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Impact Test 37.6 J
27.7 ft-lb
Instrumented Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 39.0 °C
102 °F
ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 91 %
91 %
Processing Properties Metric English Comments
Processing Temperature <= 218 °C
<= 424 °F
extrusion