Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 163 - 260 °C | 325 - 500 °F | Average value: 193 °C Grade Count:8 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 - 260 °C | 171 - 500 °F | Average value: 116 °C Grade Count:62 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 - 260 °C | 221 - 500 °F | Average value: 187 °C Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 121 - 260 °C | 250 - 500 °F | Average value: 196 °C Grade Count:10 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 - 260 °C | 444 - 500 °F | Average value: 246 °C Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 110 - 260 °C | 230 - 500 °F | Average value: 206 °C Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 199 - 260 °C | 390 - 500 °F | Average value: 238 °C Grade Count:94 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 - 260 °C | 446 - 500 °F | Average value: 251 °C Grade Count:26 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 139 - 260 °C | 283 - 500 °F | Average value: 245 °C Grade Count:73 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 232 - 260 °C | 450 - 500 °F | Average value: 243 °C Grade Count:7 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical app.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 232 - 260 °C | 450 - 500 °F | |
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC HT12-1026 Unsaturated Polyester Bulk Molding Compound BMC HT12-1026 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound BMC HT12-1024 is a high temp wear resistant molding compound designed for automotive brush holders. It is listed under Ford WS-MSD-A. It can be injection or transfer molded.Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC HT12-1027 Unsaturated Polyester Bulk Molding Compound BMC HT12-1027 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 - 260 °C | 145 - 500 °F | Average value: 129 °C Grade Count:100 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 - 260 °C | 446 - 500 °F | Average value: 250 °C Grade Count:14 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 254 - 260 °C | 489 - 500 °F | Average value: 257 °C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 232 - 260 °C | 450 - 500 °F | Average value: 251 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 174 - 260 °C | 345 - 500 °F | Average value: 191 °C Grade Count:13 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 - 260 °C | 331 - 500 °F | Average value: 196 °C Grade Count:9 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 - 260 °C | 203 - 500 °F | Average value: 119 °C Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC T45HT Automotive Grade Molding compound BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester base.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes.. |