Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Plaskolite PETG Mirror Sheet Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Nylene® 721 Nylon 6 Dry as molded. Injection molding grade. Nylene 721 is a medium impact modified nylon for fast, easy molding. Parts molded from 721 have good impact strength right out of the mold without post condi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPHC T15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | |
Eastman Eastar GN101 PETG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ISO 75 |
Solvay Engineered Polymers SEQUEL® 2300 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2300 engineered polyolefin is designed for large mold-in-color automotive interior applications that require high stiffness and dimensional stability over a broad temperature r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ISO 75-1/-2 |
Lanxess Durethan® DP BC 310 EF 000000 Nylon 6 PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ISO 75-1/-2 |
Lanxess Durethan® DP BC 310 EF 600065 Nylon 6 PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C @Thickness 6.40 mm |
145 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa PBT-R0N Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ISO 75-1,-2 |
Gromax BTE30-FN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C @Thickness 3.20 mm |
145 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C @Thickness 3.20 mm |
145 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1477 Mineral Filled, General-Purpose Polypropylene DescriptionPolyfort® FPP 1477 is a 20% mineral filled, general-purpose polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2496 is an injection molding grade mineral fortified and impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Eastman Aspira EB062 Copolyester Resin for Extrusion Blown Bottles Applications:Beverage packagingBottlesExtrusion blow moldingFood packagingPersonal care bottlesKey Attributes:Easy to extrude, cut, print and sealEffective barrier propertiesExcellent chemical resis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Eastman Eastar CN005 Copolyester, High Flow Grade Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Eastman Provista MP002 Copolymer Provista Copolymer MP002 is a resin specifically developed for extrusion into profiles for medical applications where aesthetics such as high clarity and gloss, coupled with design flexibility and e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Eastman Provista ST Copolymer Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation m.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ISO 75-2 |
Denka TH-23 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 Zytel FE3734 NC010 is an unreinforced lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | Unannealed; ISO 75-2/A |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | Unannealed; ISO 75-2/A |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
BASF Ultramid® 8270 HS BK 102 PA6 (Dry) Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM Test |
BASF Ultramid® 8270 HS PA6 (Dry) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 604 Nylon 6/6, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
A. Schulman ComAlloy Lubrilon® 604 Nylon 6/6, PTFE/Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | Unannealed; ISO 75-2/A |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 - 260 °C | 145 - 500 °F | Average value: 129 °C Grade Count:100 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH TS3020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Ashley Polymers Ashlene® 830LW Nylon 6 Basic Nylon 6, medium viscosity, lubricated for general purpose injection molding.Data provided by the manufacturer |