Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 1510 CNU White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C @Thickness 3.18 mm |
136 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 87768 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C @Thickness 3.18 mm |
136 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Nymax™ 623 Zip 5 HS Black 13 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
Ravago Manufacturing Americas Enviramid™ N1300THL BK Post Consumer Recycle Nylon 66 Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
Global GPP-2500 Polypropylene Impact Copolymer, Nucleated Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | Unannealed; ASTM D648 |
LyondellBasell Hifaxâ„¢ RTA3263EC/1 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EC/1 fractional melt flow, 1,700 MPa flexural modulus, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffn.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CMU 236 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior covered applications such as retainers in which a good stiffness/toughness balance is required.Availa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CMV 205 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive interior applications in which good surface finish and good UV resistance .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ISO 75-2/A |
ExxonMobil Exxtral™ LNU 012 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good heat resistance and good surface finish designed for fast injection molding of large electrical appliance parts.Availability.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accucomp Polypropylene CPO425BAV Automotive Approved Copolymer Expandable Grade |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accuguard Polypropylene HP0369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accuguard Polypropylene HP1362V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accutech Polypropylene Copolymer CP0437M30L Mica Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accutech Polypropylene Copolymer CP0437T40L Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accutech Polypropylene Homopolymer HP0334C30L1 Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339C10L Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accutech Polypropylene Copolymer CP0436T20L1 Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accutech Polypropylene CP0405UVV Copolymer UV Stabilized Approved to Suzuki PP-S2 Med Grey T01 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | |
Aclo Accutech Polypropylene HP0315V Homopolymer High Heat Approved to GMP.PP.013 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | Unannealed; ASTM D648 |
Multibase Multi-Flam™ 0102 Natural PP Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
Solvay Engineered Polymers SEQUEL® E3000 HMS TPO
(discontinued **) Description: SEQUEL® E3000HMS thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is spec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |