| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer | 
| Manufacturer | Global Polymers Corporation | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Global GPP-2500 Polypropylene Impact Copolymer, Nucleated.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 | 
| Melt Flow | 25           g/10 min @Load 2.16 kg, Temperature 230 °C | 25           g/10 min @Load 4.76 lb, Temperature 446 °F | L; ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 21.4 MPa | 3100 psi | Type 1 Specimen, Rate: 2"/min; ASTM D638 | 
| Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 | 
| Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 | 
| 0.534           J/cm @Temperature -30.0 °C | 1.00           ft-lb/in @Temperature -22.0 °F | ASTM D256 | |
| 0.854           J/cm @Temperature 0.000 °C | 1.60           ft-lb/in @Temperature 32.0 °F | ASTM D256 | |
| Dart Drop, Total Energy | 38.4           J @Temperature -30.0 °C | 28.3           ft-lb @Temperature -22.0 °F | 150 in/sec; ASTM D3763 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 57.8 °C | 136 °F | ASTM D648 |