Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM D648-95 |
Multibase Multi-Pro® 0710 C Brown Polypropylene Data provided by Multibase. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | Method A, flatwise, unannealed; ISO 75-1/2 |
Mytex Polymers AS172LW-01US Thermoplastic Polyolefin, Compounded AS172LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM D495 |
Nylene® 452 Nylon 6 Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Bec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PP CIQ15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Faradex MS002P PP (Europe-Africa-Middle East) LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | |
Polimeri Europa KOBLEND HI 20 PBT+PC, Impact Grade
(discontinued **) PBT elastomer modified with good impact behaviour, good stiffness, resistant to solvents. Main application fields: automotive industryUnfilled. Suitable for Injection Molding. Supplied as pellets.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 - 200 °C | 133 - 392 °F | Average value: 108 °C Grade Count:10 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C @Thickness 3.20 mm |
133 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ISO 75/Af |
Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1609 Mica Fortified Copolymer Polypropylene DescriptionPolyfort® FPP 1609 is a 10% mica fortified copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ISO 75-1, 2 |
Polyplastics Duranex® 800FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Viscosity DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ISO 75 |
Wellman Wellamid® 22LHI6 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ISO 75-93 |
Wellman Wellamid® 22LHI6 XE-NBK1 Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM D648 |
Formosa Plastics Formolene® 6144O Impact Copolymer Polypropylene Impact Copolymer for Appliance Applications Formolene® 6144O is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1609 Mica Fortified Copolymer Polypropylene DescriptionPolyfort® FPP 1609 is a 10% mica fortified copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM D648 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ISO 75-2 |
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ISO 75 |
Unipetrol PP MONSTEN® GB 005 Polypropylene Homopolymer Applications include injection molding, tapes, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | dry; ISO 75-1/-2 |
DSM Novamid® 1011CH5KR PA6 Heat Stabilized, Easy Molding Grade |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ISO 75-2/A |
Cathay PA511 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | |
BASF Procom® D 1158 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ISO 75 |
BASF Ultramid® 8253 BK-102 PA6 (Dry) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM D648 |
Ashley Polymers Ashlene® 630 Nylon 6, General Purpose A general purpose Nylon 6 resin for injection molding.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | |
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Conditioned) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM D648 |
Ashley Polymers Ashlene® 630BU Nylon 6 Black utility grade Nylon 6 for injection molding.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM-D648 |
Braskem CP 284R HECO Polypropylene Heterophasic Copolymer CP 284R is a heterophasic copolymer designed for injection molding of pails and containers with excellent stiffness/impact strength balance. This resin also exhibits excellent productivity and proce.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | ASTM D648 |
Braskem H 606 Thermoforming Polypropylene Description: H 606 is low melt flow rate homopolymer with general purpose additive package. This resin is designed for extrusion and thermoforming. H 606 presents excellent processability and high o.. |