Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 277 °C | 531 °F | ASTM D-648 |
PlastiComp Complet® LGF40-PPA Polyphthalamide, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 40% long glass fiber reinforcementInformation provided by PlastiC.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 277 °C @Thickness 6.35 mm |
531 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 277 °C | 530 °F | ASTM D648 |
Quantum PEEK 30% Carbon Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 277 °C | 531 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 277 °C | 531 °F | Annealed; ISO 75-2/Af |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 277 °C | 531 °F | ASTM D648 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 277 °C | 531 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA), 45% Glass Fiber Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 277 °C | 531 °F | Annealed; Flatwise; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 277 °C | 531 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam.. |