Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 700 °C @Thickness 2.00 mm |
1290 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East) Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by .. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
GWIT; IEC 60695-2-13 |
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 700 °C @Thickness 2.00 mm |
1290 °F @Thickness 0.0787 in |
GWIT; IEC 60695-2-13 |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
DAM; IEC 60695-2-12 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® C CM 406 FD C CM 406 Polycarbonate/ABS Blend (European Grade) Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 700 °C @Diameter 1.60 mm |
1290 °F @Diameter 0.0630 in |
IEC 60695-2-12 |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Glow Wire Test | 700 °C @Thickness 1.60 mm |
1290 °F @Thickness 0.0630 in |
Flammability Index; IEC 60695-2-12 |
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Glow Wire Test | 700 °C @Thickness 0.710 mm |
1290 °F @Thickness 0.0280 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Glow Wire Test | 700 °C @Thickness 0.710 mm |
1290 °F @Thickness 0.0280 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
Glow Wire Test | 700 °C @Thickness 0.710 mm |
1290 °F @Thickness 0.0280 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Glow Wire Test | 700 °C @Thickness 0.710 mm |
1290 °F @Thickness 0.0280 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Glow Wire Test | 700 °C @Thickness 0.900 mm |
1290 °F @Thickness 0.0354 in |
IEC 60695-2-12 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Glow Wire Test | 700 °C @Thickness 1.00 mm |
1290 °F @Thickness 0.0394 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |