Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam Soft, low compression set silicone foam often specified to meet safely-conscious requirements. UL recognized for flame retardance.Applications: Low closure-force gaskets and seals, Vibration and sh.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam Firm grade silicone sponge. UL recognized for flame retardance.Applications: Gaskets where higher closure force is available or necessary, Cushions in heavier-load applicationsGasketing and sealing.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ HT-840 Cellular Silicone Foam Extra firm grade silicone sponge. UL recognized of flame retardance.Applications: High closure-force gaskets, Press-pads where conformable imprinting support is required, such as decal lamination o.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Polyplastic TechnoTep B® 45 D Thermoplastic Elastomer, Mineral Filled High mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Polyplastic TechnoTep B® 60 A Thermoplastic Elastomer, Mineral Filled Medium mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
S&E Specialty Polymers TufFlex™ GTPO8290 Natural TPO Compound Application: An olefin based insulation & jacketing , 105°C rated compound formulated with excellent deformation characteristics. (SEW, SJEW)Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics Tecksof 2000 Conductive Fabric Over Foam Gasket Description: The Tecknit TECKSOF 2000 Series gasket consists of conductive fabric over foam and has been designed to meet today’s commercial EMI shielding applications demands where wide tolerance .. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Elastamax™ HTE 3050 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Polyplastic TechnoTep B® 65 A Thermoplastic Elastomer, Mineral Filled High mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ HT-870 Cellular Silicone Foam Gasketing and sealing rating is JMLU-2 (Listed) per UL 157. No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B5500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -55.0 - -16.0 °C | -67.0 - 3.20 °F | Average value: -34.1 °C Grade Count:16 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Brittleness Temperature | <= -55.0 °C | <= -67.0 °F | |
Sibur O-55 Compound 1182 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Saint-Gobain Tygon® E-1000 Ultra-Soft Laboratory Tubing Soft and flexible, Tygon® E-1000 Non-DEHP laboratory tubing delivers the same performance in a formulation that contains non-DEHP [Bis (2-ethylhexyl) phthalate] plasticizers. The market demand a.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3500-45 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3501-45-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D 746 |
Zylog Neoplast® 187 FT EB Thermoplastic Vulcanizate Neoplast 187 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 4510/R Flexible PVC, Injection Molding for Footwear Vamp Boots with Rubber |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 46/T Flexible PVC, Injection Molding for Footwear Vamp boots |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 66/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | XT<sub>b</sub>; ASTM D746 |
Colorite Polymers Elastichem 5011TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Colorite Polymers MULTICHEM™ 6014 Vinyl-Urethane Blend Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 45/1 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
AlphaGary Garaflex™ E 50-10 B Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable90°C rated non-migrating jacket compound for Mil C 17G |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Colorite Polymers 6014 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | <= -55.0 °C | <= -67.0 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |