Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
PolyOne Synprene™ RT-5190 RoHS Black Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3775 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WR7400L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
LyondellBasell Microthene® F FN50100 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Multibase Multi-Flex® D 3902 MRS TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Multibase Multi-Flex® A 9002 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex ELEXAR® EL 8614 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3500-60 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3501-60-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1654A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | JIS K6301 |
Toyobo PELPRENE™ S9002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D 746 |
Zylog Neoplast® 240 FT EB Thermoplastic Vulcanizate Neoplast 240 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ISO 974 |
Chengdu Polyster FH7560 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H7560 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 54 Flexible PVC, Injection Molding for Footwear Boots - sandshoes |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
Fainplast Compounds GS 55/UV Flexible PVC, Injection Molding for Transparent Technical Items Outdoor protections for switches anti-UV |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Colorite Polymers Weatherflex™ CS1536WX (NTL70B) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 5010 Flexible PVC, Lead Free Gaskets for frames |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
AlphaGary Garaflex™ O 9949 RA Olefinic Thermoplastic Elastomer Garaflex™ O is a flame retarded, olefinic thermoplastic elastomer105°C rated flame retardant olefinic TPE for flat ribbon cable and heat tracing cable |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Advanced Polymer Alloys Alcryn® 2180 BK Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D-746 |
Axiall 16782 Wire & Cable Flexible PVC Non-lead stabilized, 90C jacketing compound with excellent low temperature performance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D726 |
Arkema Group LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. Main applicationsLOTADER 3210 is a versatile adhesive for extrusi.. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D726 |
Arkema Group LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3430 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3430 is a versatile adhesive for extrusion coating or lam.. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D726 |
Arkema Group LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 4210 is a versatile adhesive for extrusion coating or lam.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | Plasticizer conc. in vinyl film 70 phr; ASTM D746 |
BASF Palatinol® 11P-E (DUP) Linear Phthalate Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing .. |