Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3904 Polyvinyl Chloride, Flexible (PVC, Flexible) A Clear-Frosted PVC compound formulated specifically for FDA extrusion and Molding applications.The physical properties listed below, are typical values obtained on compression molded sheets and tes.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W2301 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Low temp embrittlement; ASTM D746 |
Rogers Corporation Poron® 4701-50-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne Geon™ HC 2155 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2155 is a 55 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2155 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R1211P Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Asia Pacific) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD801A PPE-TPE (Asia Pacific) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD835 PPE-TPE Flexible, low odor, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD861A PPE-TPE Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | |
Sibur NGP 40-32 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex APEX® 3210-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex APEX® 3800-75 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor .. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex APEX® 583 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: General Purpose Uses: Tubing; Wire Jacketing Agency Ratings: UL 498; UL 62 Wire Types: SPT-1; SPT-2 Processing Method: Injection MoldingForms: PelletsInformation Prov.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex APEX® 94-A0098A-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3500-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3500-75NT Polyvinyl Chloride Elastomer Features: Good Thermal Stability; Recyclable Material; Good Weather Resistance; Ultra High Molecular Weight Uses: Medical/Healthcare Applications; Pump Parts; Tubing Agency Ratings: FDA Unspecified .. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ISO 974 |
Chengdu Polyster CH7563 Thermoplastic Polyether-ester Elastomer (TPEE) Poly-basic block copolymer. Good compatibility with PBT, PET and PA. For blending with PBT, PET and PA to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Temperature Retraction, TR-10 |
Dow Nordel® IP 4640 Molded Brake Cup FormulationNordel® IP 4640 |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Temperature Retraction, TR-10 |
Dow Nordel® IP 5565 Heat Resistant Peroxide Cured FormulationNordel® IP 5565 |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 61/R Flexible PVC, Injection Molding for Footwear Oil resistent bottom boots |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Colorite Polymers 7077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 55 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D2137 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2775 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D-746 |
Axiall 10750 Wire & Cable Flexible PVC General purpose 75C jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |