Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Rynite® GW520CS NC010 PET
(Unverified Data**) Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) Zytel® 70G30HSL BK039B is a 30% glass reinforced, heat stabilized, black nylon 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.710 mm |
284 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG5 (Dry) 25% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness >=0.710 mm |
284 °F @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP1000D PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness >=1.50 mm |
284 °F @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000D PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness >=0.710 mm |
284 °F @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness >=3.00 mm |
284 °F @Thickness >=0.118 in |
|
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness >=0.710 mm |
284 °F @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness >=3.00 mm |
284 °F @Thickness >=0.118 in |
|
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness >=1.50 mm |
284 °F @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2306FI PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness >=3.00 mm |
284 °F @Thickness >=0.118 in |
|
LG Chemical Lupox® GP2306FG PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness >=1.50 mm |
284 °F @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2306FY PBT+GF30% Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL746B |
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.710 mm |
284 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-HG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® TV4 240 S PBT-20% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.800 mm |
284 °F @Thickness 0.0315 in |
ALL |
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
ALL |
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 2.00 mm |
284 °F @Thickness 0.0787 in |
ALL |
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 1.60 mm |
284 °F @Thickness 0.0630 in |
|
Eurostar Starflam RF0057P PA66/6, 25% Glass Filled, Injection Molded Starflam RF0057P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.800 mm |
284 °F @Thickness 0.0315 in |
|
Eurostar Starflam RF0077E PA66, 35% Glass Filled, Injection Molded Starflam RF0077E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as RF1007Z270)Information provided by Polymer T.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.800 mm |
284 °F @Thickness 0.0315 in |
|
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |