Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-HG5 Nylon 6-25% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL746B |
Mitsubishi Xantar® 18 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® 27 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® 27 U Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® F 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® F 23 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 19 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 23 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® F 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 19 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 23 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® MX 1082 Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 0.800 mm |
257 °F @Thickness 0.0315 in |
|
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
|
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-HG3 (Dry) 15% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
|
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
|
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**) Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® F 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |