Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Electrical = 125 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
UL RTI, Electrical 125 °C
<br>@Thickness 5.99 mm
257 °F
<br>@Thickness 0.236 in
UL 746
Polymer Resources NY6-GP1 General Purpose Nylon 6
General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
UL RTI, Electrical 125 °C
<br>@Thickness 0.800 mm
257 °F
<br>@Thickness 0.0315 in
UL 746
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized
General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow
Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t..
UL RTI, Electrical 125 °C
<br>@Thickness 1.50 mm
257 °F
<br>@Thickness 0.0591 in
UL 746
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow
Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted..
UL RTI, Electrical 125 °C
<br>@Thickness 1.50 mm
257 °F
<br>@Thickness 0.0591 in
UL 746
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow
Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow
Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on..
UL RTI, Electrical 125 °C
<br>@Thickness 1.50 mm
257 °F
<br>@Thickness 0.0591 in
UL 746
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release
Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
PolyOne Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)
These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized
General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades..
UL RTI, Electrical 125 °C
<br>@Thickness 5.99 mm
257 °F
<br>@Thickness 0.236 in
UL 746
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized
General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades..
UL RTI, Electrical 125 °C
<br>@Thickness 1.50 mm
257 °F
<br>@Thickness 0.0591 in
UL 746
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples...
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release
Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
UL RTI, Electrical 125 °C
<br>@Thickness >=1.60 mm
257 °F
<br>@Thickness >=0.0630 in
LG Chemical LUCON SP9306FL sPS+MF
Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 ..
UL RTI, Electrical 125 °C
<br>@Thickness >=1.50 mm
257 °F
<br>@Thickness >=0.0591 in
LG Chemical Lupoy 1301EP22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Electrical 125 °C
<br>@Thickness >=1.50 mm
257 °F
<br>@Thickness >=0.0591 in
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Electrical 125 °C
<br>@Thickness >=3.00 mm
257 °F
<br>@Thickness >=0.118 in
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Electrical 125 °C
<br>@Thickness 1.60 - 1.70 mm
257 °F
<br>@Thickness 0.0630 - 0.0669 in
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin
Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Electrical 125 °C
<br>@Thickness 0.810 mm
257 °F
<br>@Thickness 0.0319 in
UL 746
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced
Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex
UL RTI, Electrical 125 °C
<br>@Thickness 0.810 mm
257 °F
<br>@Thickness 0.0319 in
UL 746
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced
Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex..
UL RTI, Electrical 125 °C
<br>@Thickness 0.750 mm
257 °F
<br>@Thickness 0.0295 in
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
UL RTI, Electrical 125 °C
<br>@Thickness 0.800 mm
257 °F
<br>@Thickness 0.0315 in
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
UL RTI, Electrical 125 °C
<br>@Thickness 1.50 mm
257 °F
<br>@Thickness 0.0591 in
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded
PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
DAM; UL 746B
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66 &nbsp;(Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
UL RTI, Electrical 125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..