Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® 2014R PC (Europe-Africa-Middle East) LEXAN 2014R is a medium viscosity flame retardant grade, This material contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region... |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
PTS Tristar® PC-10R-(V20) 20 MFI UV Stabilized Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® HF1140R PC (Europe-Africa-Middle East) LEXAN HF1140R is a high flow grade. This material is especially designed for applications that require thin wall sections and high flow lengths. FDA food contact compliant in limited colors.Effect.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
PTS Tristar® PC-10R-CL02(V38) 38 MFI Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific) 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746 |
Styron EMERGEâ„¢ 4610-10 Polycarbonate EMERGEâ„¢ PC 4610-10 advanced resin is formulated to deliver both outstanding clarity and enhanced ignition resistance while maintaining excellent physical properties and processability. Applica.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746 |
Styron EMERGEâ„¢ 4630-10 Polycarbonate EMERGEâ„¢ PC 4630-10 advanced resin is formulated to supply both excellent ultraviolet stability and enhanced ignition resistance while maintaining excellent physical properties and processabilit.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746 |
Styron EMERGEâ„¢ 8600-20 Polycarbonate EMERGEâ„¢ PC 8600-20 is a translucent, ignition-resistant and easy flow polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global .. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific) 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.47 mm |
257 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® L-1250ZW Extrusion Grade Polycarbonate Resin Information provided by Teijin Chemicals Ltd. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
Covestro Makrolon® 2258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
Covestro Makrolon® 2407 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officia.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
|
Covestro Makrolon® 2858 Polycarbonate, Injection Grade Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
|
Covestro Makrolon® 6255 Polycarbonate, Flame Retardant, High Productivity, Mold Release Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.10 mm |
257 °F @Thickness 0.0433 in |
|
Covestro Makrolon® 6465 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offici.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | |
Covestro Makrolon® 6555 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a.. |
|||
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
Covestro Makrolon® ET3227 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |