Deflection Temperature at 0.46 MPa (66 psi) 300 °C
572 °F
Unannealed; ASTM D648
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
>= 572 °F
LATI Laticonther 88/10 GR/50 PEEK, 50% Graphite Reinforced
High thermal conductivity product based on Polyetheretherketone (PEEK). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Deflection Temperature at 0.46 MPa (66 psi) 300 °C

@Thickness 3.20 mm
572 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK
LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am..
Deflection Temperature at 0.46 MPa (66 psi) 300 °C
572 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel..
Deflection Temperature at 0.46 MPa (66 psi) 300 °C
572 °F
ISO 75
Eurotec® Tecomid® NT40 GR15 NL HS PPA, 15% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Deflection Temperature at 0.46 MPa (66 psi) 300 °C
572 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..