Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | Unannealed; ASTM D785 |
Ravago Manufacturing Americas Hylon® N1200THL BK Nylon 6/6 Available in North America Additive: Heat Stabilizer, Impact Modifier and Lubricant Features: Lubricated, Impact Modified and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources NY66-IM1 Nylon 66, Medium Impact Modified Nylon 66, Medium Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are te.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources NY66-IM1-[color]-H Nylon 66, Medium Impact Modified, Heat Stabilized Nylon 66, Medium Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Ny.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources NY66-IM1-[color]H Nylon, Medium Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources NY6-M25G15 Nylon 6, 25% Mineral, 15% Glass Reinforced Nylon 6, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gra.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF33 BK 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PBT GF30 HR BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Hydrolysis ResistantAppearance: BlackInformation provided by TP Composites, In.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PBT/ABS GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Plastics Group Polifil® 625L Nylon 6/6 (DAM) Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Clariant Renol 6601L Nylon 66, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |