Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
RheTech Products P104-00 Polypropylene, Natural Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
RheTech Products HP520-00 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Ineos 3950 Polypropylene Impact Copolymer Grade 3950 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP1-2002AF Food Grade Polypropylene Homopolymer A 20 melt injection molding grade of Polypropylene homopolymer with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP1-2002ARX Biocompatible Polypropylene Homopolymer A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Ineos L34N-00 Polypropylene Impact Copolymer Grade L34N-00 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HIPS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HIPS GF50 50% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Plastics Group Polifil® GFABS-20 20% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Ensinger Hydex™ 301 Rigid Polyurethane (PU) Hydex™ 301 is clear totally rigid polyurethane. It combines excellent clarity when polished with a broad range of chemical resistance and outstanding practical toughness. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648 |
Dow 5D49 Polypropylene Resin DOW 5D49 is intended for use fiber spinning processes. It is well suited for spunbond non-woven applications.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braske.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Aaron Industries AVPP HOMO 200-1 Virgin Polypropylene A virgin polypropylene specifically designed for all injection molding applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Asahi Kasei Thermofil D-10FG-1101 10% Glass Fiber Reinforced, ABS Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Asahi Kasei Thermofil P-20TC-Y118 20% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Aaron Industries AAROLENE® AVPS HIPS 100-3 MELT 14 Virgin HIPS Resin A virgin, high impact polystyrene, natural in color, specifically designed for injection molding applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
Spartech EP6120 Filled and Reinforced Copolymer Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength.. |