Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648-56 |
Rotuba 855, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycolac® GPM5500F ABS (Europe-Africa-Middle East) CYCOLAC GPM5500F is a multi purpose injection moulding grade, providing a favourable balance of engineering properties and is FDA and European Directive 2002/72/EC
(FCEU) compliant for food contac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycolac® GPM5500U ABS (Europe-Africa-Middle East) CYCOLAC GPM5500U is a UV stabilized multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500U has a wide processing window. It is recommended.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycolac® MG94 ABS Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Network Polymers NPP 25-2002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Reliance Industries Polypropylene - Suzorite mica (untreated) filler Information provided by Reliance Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Asia Pacific) LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Centrex® 813 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Flint Hills P5C4K-089 Random Copolymer Polypropylene Features: Good clarity. Product does not contain animal derived components. Phthalate-freeApplications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Lustran® 1152 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Lustran® 556 Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoforming |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Lustran® LGM Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
LyondellBasell Hostacomâ„¢ BG722AC Polypropylene Copolymer Description: Hostacomâ„¢ BG722AC medium high melt flow, 1,700 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer is designed with an excellent balance of stiffness, impact r.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hostacomâ„¢ BR712GC Polypropylene Copolymer Description: Hostacomâ„¢ BR712GC conventional melt flow, 1,300 MPa flexural modulus, UV-stabilized, mineral-filled polypropylene copolymer has an excellent balance of stiffness, impact and weathe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON MX01767C PP LNP* STAT-KON* MX01767C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8007 Availability: North AmericaForms: PelletsFeatures: General Purpose and High FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® ABS FR AS BN Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM Test |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Eastman Eastar DN003 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | unannealed; injection molded; ASTM D648 |
Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | annealed; ASTM D648 |
Arkema Group Solarkote® A200 Acrylic Superior UV protection and weatherability, ASTM Classification PMMA 0233V1Information provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | unannealed; injection molded; ASTM D648 |
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Ineos H19G-00 Polypropylene Homopolymer This is a homopolymer designed for extrusion processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsContinuous Filament YarnBCFSta.. |