Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648-06 |
Objet FullCure® 870 Vero Black Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 77.8 °C | 117 - 172 °F | Average value: 54.8 °C Grade Count:14 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.2 °C | 117 °F | ASTM D648 |
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. Regulatory Status: GA564189 meets the .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | |
Teknor Apex TEKRON® 4300-B88 2UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | |
Teknor Apex TEKRON® 4300-B88 UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, MDI-based 2-Component Liquid System 0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 50.0 °C | 117 - 122 °F | ASTM D648-98c |
DSM Somos® 9420 Epoxy Resin for Stereolithography DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.2 °C | 117 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.2 °C | 117 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | |
Arkema Group Orgalloy® LE 60THM Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in rigidity than LE 6000. For film, hollow vessel blow moldi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.2 °C | 117 °F | ASTM D648 |
Aclo Accucomp Polyethylene HD0205L High Density |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 76.0 °C | 117 - 169 °F | Average value: 64.0 °C Grade Count:21 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 204 °C | 117 - 399 °F | Average value: 156 °C Grade Count:4 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 100 °C | 117 - 212 °F | Average value: 77.4 °C Grade Count:7 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |