Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C

@Thickness 3.18 mm
106 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Maxxam™ FR MF5420-0013 FR Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
Deflection Temperature at 0.46 MPa (66 psi) 41.1 - 88.9 °C
106 - 192 °F
Average value: 72.5 °C Grade Count:81
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2210 H SK LDPE
Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2410 T LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2420 F LDPE
Film, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2420 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2420 K LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2425 K LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2426 F LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2441 D LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2003 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1800 S LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1804 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1810 D LDPE
Blow moldings, sheet, profile, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1810 E LDPE
Blow moldingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1810 H LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1812 D LDPE
Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1812 E LDPE
Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1840 D LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1840 H LDPE
Blow moldings, injection moldings, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE
LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C

@Thickness 3.20 mm
106 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C

@Thickness 3.20 mm
106 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C

@Thickness 3.20 mm
106 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C

@Thickness 3.20 mm
106 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C

@Thickness 3.20 mm
106 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 341 Ionomer
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 - 45.0 °C
106 - 113 °F
Average value: 42.6 °C Grade Count:5
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 1800 H LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
LyondellBasell Lupolen® 2424 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 41.0 - 45.0 °C
106 - 113 °F
Average value: 42.9 °C Grade Count:17
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..