LyondellBasell Lupolen® 2420 F LDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer LyondellBasell
Trade Name Lupolen®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LyondellBasell Lupolen® 2420 F LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Film, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
Water Absorption 0.010 %
0.010 %
Moisture Absorption at Equilibrium 0.010 %
0.010 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.0 MPa
1600 psi
Elongation at Break >= 50 %
>= 50 %
Elongation at Yield 14.5 %
14.5 %
Tensile Modulus 0.260 GPa
37.7 ksi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 230 µm/m-°C

@Temperature 20.0 °C
128 µin/in-°F

@Temperature 68.0 °F
Melting Point 111 °C
232 °F
Deflection Temperature at 0.46 MPa (66 psi) 41.0 °C
106 °F
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Oxygen Index 17 %
17 %
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.3

@Frequency 100 Hz
2.3

@Frequency 100 Hz
2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
Dissipation Factor 0.00020

@Frequency 100 Hz
0.00020

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V