Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | Unannealed; ASTM D648 |
Multibase Nylex™ 1230 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
Network Polymers NPP 20-0202 Description: Random Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CY203 PC+ABS (Europe-Africa-Middle East) Cycoloy* CY203 is a industrial quality PC+ABS flame retardant grade for injection moulding applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C @Thickness 3.20 mm |
176 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Geloy XTWE280 ASA Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | Unannealed; ISO 75-2/C |
Pasargad Polymer Peyvand Pasalen 3P-M3520B Polypropylene, 20% EPDM Filled Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components BumperAutomotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
LyondellBasell Alathon® M6580 High Density Polyethylene ApplicationsALATHON M 6580 is a narrow molecular weight distribution homopolymer that enhances processability and stiffness, exhibits excellent color, low odor and good processing stability. Typica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | Unannealed; ASTM D648 |
Global PP-3375-RM Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-fabricsInformation provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
LG Chemical SEETEC T3410 Polypropylene Random Terpolymer Features: Seetec T3410 is a polypropylene-ethylene-butene random terpolymer designed for the production of Transparent Film and Expandable PP for low seal temperature and high impact strength. It of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | |
Kraton® G1650 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
LyondellBasell Astryn 75A6-2 Polypropylene Copolymer, 20% Calcium Carbonate Key Features: conventional melt flow, medium modulus, mineral-filled polypropylene copolymer, high impact, excellent chemical resistance, excellent aesthetics, high gloss, good colorability, good pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
LyondellBasell Hifaxâ„¢ ETA-4161UV Thermoplastic Olefin Resin Key Features: fractional melt flow, medium high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good melt strength, excellent weatherabili.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
Lavergne VYSTYRENE PS 3901 High Impact Polystyrene Vystyrene PS 3901 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-2 |
Borealis Borclear™ RF366MO Polypropylene Random Copolymer for Injection Molding Borclear™ RF366MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-2 |
Borealis HH450MO Polypropylene HH450MO is a polypropylene homopolymer intended for injection molding. This grade is especially suitable for high-speed injection molding of articles demanding easy flow. This polymer is a CR (cont.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3708U UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 3708U is a 20% CAC03 filled UV stable copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-1/-2 |
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM-D648 |
CTC X-PRO CTC PP1035 Polypropylene Homopolymer X-PRO PP 1035 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 4128 black 9221 PA610 Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® BM6574 BK316 TPC-ET
(Unverified Data**) Hytrel® BM6574 is a 65 nom. Shore D, plasticiser free high performance resin for blow molding and extrusion; it shows ageing resistance up to 150°C, and excellent mechanical properties at elevated.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
Diamond Polymers NPP20-0201 Random Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | |
BASF Novolen® 2448 L Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
Cheng Yu Plastic IPS600UV Flame Retardant HIPS |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-1/-2 |
DSM Arnitel® UM551 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |