Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Index of Compound 8.0 - 10 g/10 min
8.0 - 10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 102
102
ASTM D785
Tensile Strength, Yield 37.4 MPa
5420 psi
ASTM D638
Flexural Yield Strength 63.7 MPa
9250 psi
ASTM D790
Izod Impact, Notched 0.883 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Flammability, UL94 V-0
V-0