Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
120°C/h; ISO 75/1
Polykemi AB SCANAMID 66 A12^ F25 NH10 Nylon 66, Glass Fiber Reinforced, Flame Retardant
Information provided by Polykemi AB
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened
Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Polymer Resources NY66-G13-[color]-H Nylon 66, 13% Glass Reinforced, Heat Stabilized
Nylon 66, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Polymer Resources NY66-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized
Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
Deflection Temperature at 0.46 MPa (66 psi) 249 - 271 °C
480 - 520 °F
Average value: 258 °C Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu..
Deflection Temperature at 0.46 MPa (66 psi) 249 °C

@Thickness 3.20 mm
480 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP RX05487 PA 66
LNP* LUBRICOMP* RX05487 is a compound based on Nylon 66 containing 10% Aramid Fiber, 10% Lubricant. Added features of this material are: Low Warpage, Wear Resistant.
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6/6 CM40 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural ..
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6/6 GF/M25HS L BK 25% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight and Mineral Filler, 25% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66
LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific)
LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66
LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead.
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Clariant PA123G25 Nylon 66, 25% Glass Fiber, Impact Modified, Heat Stabilized
Data provided by Clariant Masterbatches
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET
45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd.
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Adell AL-18 Nylon 66, 40% Glass Reinforced; Mineral Filled
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) >= 249 °C
>= 480 °F
ASTM D648
Adell AR-18 Nylon 66, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) >= 249 °C
>= 480 °F
ASTM D648
Adell AR-37 Nylon 66, 35% Glass Reinforced
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) >= 249 °C
>= 480 °F
ASTM D648
Adell AR-38 Nylon 66, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Adell AT-14 Nylon 66, 20% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Ashley Polymers Ashlene® 528LSB2-20G Nylon 66, 20% Glass Reinforced
A UV Stabilized 20% glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufac..
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Adell AJ-37 Nylon 66, 35% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) >= 249 °C
>= 480 °F
ASTM D648
Adell AR-17 Nylon 66, 35% Glass Reinforced
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Adell AT-17 Nylon 66, 35% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Adell AT-34 Nylon 66, 20% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.