Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 100 °C |
6.22 µin/in-°F @Temperature 68.0 - 212 °F |
|
International Mold Steel Daido DRM1 Matrix High-Speed Steel This tough matrix type high speed tool steel features high hardness and high tough Matrix type high speed tool steel vastly surpasses hot work die steels. DRM1 improves hot and warm die life by its .. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 260 °C |
6.22 µin/in-°F @Temperature 68.0 - 500 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 1.5" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature -100 - 121 °C |
6.22 µin/in-°F @Temperature -148 - 250 °F |
|
Latrobe MP35N® Alloy MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties - ultra high strength, toughness, ductility, and outstanding corrosion resistance. The .. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 260 °C |
6.22 µin/in-°F @Temperature 68.0 - 500 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 1.25 RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 260 °C |
6.22 µin/in-°F @Temperature 68.0 - 500 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 316 °C |
6.22 µin/in-°F @Temperature 68.0 - 601 °F |
|
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 316 °C |
6.22 µin/in-°F @Temperature 68.0 - 601 °F |
|
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 316 °C |
6.22 µin/in-°F @Temperature 68.0 - 601 °F |
|
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 316 °C |
6.22 µin/in-°F @Temperature 68.0 - 601 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 400 °C |
6.22 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec MZ 429 Zirconia, ZrO2-Y2O3 MZ 429 is a yttria-stabilized zirconia ceramic. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 38.0 - 260 °C |
6.22 µin/in-°F @Temperature 100 - 500 °F |
|
Crucible Compaction Metals CPM® VIM CRU® 20® CPM® VIM CRU® 20® is a vacuum induction melted, cobalt-free super high speed steel manufactured by the Crucible Particle Metallurgy (CPM®) process. VIM CRU processing is designed to meet the cle.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 98.9 °C |
6.22 µin/in-°F @Temperature 68.0 - 210 °F |
|
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel BÖHLER K340 ISODUR is a universal cold work tool steel with which you‘ll be making money and just when blanking coins, but also when: blanking, cutting, cold rolling, extruding, deep drawing and b.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 600 °C |
6.22 µin/in-°F @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER S290 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 400 °C |
6.22 µin/in-°F @Temperature 752 °F |
|
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 400 °C |
6.22 µin/in-°F @Temperature 752 °F |
|
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 25.0 - 50.0 °C |
6.22 µin/in-°F @Temperature 77.0 - 122 °F |
|
Carpenter Chrome Core® 8 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 22.0 - 260 °C |
6.22 µin/in-°F @Temperature 71.6 - 500 °F |
|
Carpenter Custom 450® Stainless Steel, 25 mm Bar, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 200 °C |
6.22 µin/in-°F @Temperature 392 °F |
|
Ceramic Process Systems AlSiC-10, 54 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 500 °C |
6.22 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 22.0 - 260 °C |
6.22 µin/in-°F @Temperature 71.6 - 500 °F |
|
Carpenter Custom 455® Stainless Steel, Annealed, 1.27 mm Strip Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.22 µin/in-°F @Temperature 68.0 - 199 °F |
|
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276 AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encount.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 288°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC Allegheny Ludlum Type 420HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 316 °C |
6.22 µin/in-°F @Temperature 68.0 - 601 °F |
|
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Annealed Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 316°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 482°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 100 °C |
6.22 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel CREUSABRO® 8000 High Performance Wear Resistant Steel Description: CREUSABRO® 8000 is a high performance wear resistant steel, exhibiting a wear resistance of 50% higher than that of conventional 500 HB water quenched steel. CREUSABRO® 8000 is using .. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 260 °C |
6.22 µin/in-°F @Temperature 68.0 - 500 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 6" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°.. |