Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 29.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 29.0 µm/m-°C

@Temperature <=150 °C
16.1 µin/in-°F

@Temperature <=302 °F
ISO E 831
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced
Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol..
CTE, linear 29.0 µm/m-°C

@Temperature 0.000 - 100 °C
16.1 µin/in-°F

@Temperature 32.0 - 212 °F
x direction; IPC TM-650 2.4.24
Arlon CuClad 217 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 217 uses a low fiberglass/PTFE ratio to provide the lowest dielectric constant and dissipation factor available in fiberglass reinforced PTFE based laminates. Together, these properties offe..
CTE, linear 29.0 µm/m-°C

@Temperature 0.000 - 100 °C
16.1 µin/in-°F

@Temperature 32.0 - 212 °F
y direction; IPC TM-650 2.4.24
Arlon DiClad 870 PTFE/Woven Fiberglass Laminate
Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch..
CTE, linear 29.0 µm/m-°C

@Temperature -50.0 - 30.0 °C
16.1 µin/in-°F

@Temperature -58.0 - 86.0 °F
3M Scotch-Weld™ DP-100NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP-100NS is a two-part adhesives offering fast cure and machinability.Information provided by 3M
CTE, linear 29.0 µm/m-°C

@Temperature 0.000 - 120 °C
16.1 µin/in-°F

@Temperature 32.0 - 248 °F
100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
CTE, linear 29.0 µm/m-°C

@Temperature 40.0 - 125 °C
16.1 µin/in-°F

@Temperature 104 - 257 °F
As Molded; ASTM E831
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards
Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and ..
CTE, linear 29.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled  (discontinued **)